3D Scanning

Not 100% sure what the problem is but the blue line must have been the Z+ direction while printing
Green shows how nice it can be , red shows the spots with the most problems.
My guess is the moisture level of the powder is slightly too high, which causes clumps to form along the Z-axis when transitioning to the next layer.
This could potentially also be prevented by adding chamfers or radii to the sharp corners.
Or try the horizontal orientation , will see in the second try.IMG_20260617_172941.jpg
 